TECHNICAL SPECIFICATIONS
Consumption and drying time: The thickness of the technological coating layer is not more than 0.6 mm, the drying time is from 12 to 24 hours. The vulcanization period of each layer from the passage of the tool is 0.5 – 12 hours. The material consumption rate for a single–layer coating is 1.54 liters per 1 m2 with a coating thickness of 1 mm.
Method of application: it is applied to the surface using an airless spray gun or brush.
PRODUCT MODIFICATIONS
1. TLN Ceramic (S) is intended for industrial and domestic use as thermal insulation of metal, plastic, concrete surfaces, and operating temperatures from -60°C to +200°C (short-term +260 °C).
2. TLN Ceramic (F) is intended for industrial, construction and domestic use in as thermal insulation of external and internal surfaces of buildings and structures with operating temperatures from -60 °C to +150 °C.
3. TLN Ceramic (H) is designed for industrial applications as thermal insulation of surfaces with operating temperatures from -30 °C to +750 °C.
4. TLN Ceramic (S NC) is designed for industrial and domestic use as thermal insulation of metal, plastic, concrete surfaces, and operating temperatures from -60 °C to +200 °C (short-term +260 °C). It includes antiperene additives that give the coating nonflammable properties.
5. TLN Ceramic (F NC) is intended for industrial, construction and domestic use as thermal insulation of external and internal surfaces of buildings and structures with operating temperatures from -60 °C to +150 °C. It includes antiperene additives that give the coating nonflammable properties.